Part of the humanoid robot
Bearing
The crossed roller bearing that carries the joint's load while it turns.
The step: Crossed roller bearing · Motors and drives
Ring forging in 100Cr6-class bearing steel, turning, through-hardening to 58 to 64 HRC, grinding, crossed-roller assembly. Output: crossed roller bearing, 50 to 70 mm bore.
Made from
Goes into
The map, filtered to who makes this.
The humanoid robot, with the bearing lit
How it is made4 steps
bearing steel tube or forged ringcrossed roller bearing
- 1
Cutting the ring blanks
Rings are cut from bearing-steel tube on a lathe, a little larger than the finished size.
Detail
- Goes in
- bearing steel tube or forged ring
- Comes out
- soft ring blanks
- Equipment
- lathe or CNC turning machine
- Why it matters
- The ring shrinks in heat treatment, so it is cut oversize on purpose.
- Source
- acorn-ind.co.uk · secondary, read 2026-11-09
- 2
Hardening and tempering
The rings are heated for several hours, dropped into oil to harden them, then warmed again more gently so they are not brittle.
Detail
- Goes in
- soft ring blanks
- Comes out
- hardened rings
- Equipment
- heat-treating furnace, oil quench bath, tempering oven
- Why it matters
- Hardening alone leaves the rings brittle, so they are warmed again to temper them before they are used.
- Numbers
- hardening furnace temperature: up to 850 degrees C (acorn-ind.co.uk · secondary)
- tempering temperature: about 150 degrees C (acorn-ind.co.uk · secondary)
- Source
- acorn-ind.co.uk · secondary, read 2026-11-09
- 3
Grinding the raceways
Grinding wheels bring the hardened rings to final size and give the V-shaped tracks the rollers run in their smooth finish.
Detail
- Goes in
- hardened rings
- Comes out
- finished rings
- Equipment
- bearing grinding machines
- Why it matters
- Grinding sets the accuracy of the finished bearing.
- Source
- nsk.com · primary, read 2026-11-09
- 4
Assembly with crossed rollers
Short rollers are laid in the V-groove, each one at a right angle to the next, with a spacer between every pair. The two halves of the split ring are then closed around them and fixed.
Detail
- Goes in
- finished rings, rollers, spacer retainers
- Comes out
- crossed roller bearing
- Equipment
- assembly bench; the page read does not describe the tooling
- Why it matters
- Crossing the rollers lets one thin bearing take loads from every direction, which is why a robot joint needs only one. Because the ring is split, the tightness of the bearing can be set at assembly.
- Source
- tech.thk.com · primary, read 2026-11-09
Not published (3)
- ring forging and the 58 to 64 HRC ring hardness named in the recipe step: no page read at this step gives them
- how the rollers are made and sorted: not on any page read
- final inspection and the accuracy grades of crossed roller bearings: not opened here
Who makes it, by country107 on the index
- China59
- Japan16
- United States13
- Taiwan4
- Germany4
- South Korea2
- India2
- France1
- Spain1
- Austria1
- and 2 more countries
By result
- OSC: Allied owner26
- OSC: Owner unclear23
- OSC: Covered-nation owner46
- No record12
Results under OSC foreign influence. What each result means
Where they are
Makers on the index
All 107 on the map →- American Roller Bearing CompanyUnited StatesOSC: Owner unclear
- Asahi (Asahi Seiko)Kawasaki, JapanOSC: Owner unclear
- AST BearingsUnited StatesOSC: Owner unclear
- Aurora Bearing CompanyUnited StatesOSC: Allied owner
- AVIC Harbin Bearing (中航哈尔滨轴承)Harbin, ChinaOSC: Owner unclear
- Bosch RexrothTaoyuan, TaiwanOSC: Allied owner
- BY BearingsLuoyang, ChinaOSC: Covered-nation owner
- C&U GroupShanghai, ChinaOSC: Covered-nation owner
- CCTY Bearing CompanyZhenjiang, ChinaOSC: Owner unclear
- Changjiang Bearing (长江轴承 CJB)Chongqing, ChinaOSC: Covered-nation owner
- Changsheng Bearings (CSB)Jiaxing, ChinaOSC: Covered-nation owner
- Changzhou NRB CorporationChangzhou, ChinaOSC: Covered-nation owner