Physical AI · Battery pack
Cathode and anode materials
LFP (hydrothermal or solid state) or NMC precursor to cathode powder; graphite anode. Output: active materials.
Goes into
The map, filtered to who makes this.
How it is made4 steps
Ni, Mn and Co sulfates, carbonate and hydroxide solutions, watersynthetic graphite
- 1
Precipitating the cathode precursor
Nickel, manganese and cobalt salts dissolved in water are stirred in a heated tank with a second solution, and the metals fall out together as fine solid particles.
Detail
- Goes in
- Ni, Mn and Co sulfates, carbonate and hydroxide solutions, water
- Comes out
- precursor particles in liquid
- Equipment
- continuous stirred tank reactor
- Why it matters
- The three metals have to come out of solution together and evenly; the particle made here sets the shape of the finished cathode powder. · our reading
- Numbers
- Source
- osti.gov · primary, read 2026-11-09
- 2
Filtering, washing and drying
The particles are separated from the liquid, washed several times and dried to a powder.
Detail
- Goes in
- precursor particles in liquid
- Comes out
- dry precursor powder
- Equipment
- rotary vacuum filter and spray dryer
- Why it matters
- Washing removes the leftover salts before the powder is fired. · our reading
- Source
- osti.gov · primary, read 2026-11-09
- 3
Mixing with lithium and firing
The dry powder is mixed with a lithium salt and fired in a kiln, where the lithium reacts into the particles.
Detail
- Goes in
- dry precursor powder, lithium carbonate or hydroxide
- Comes out
- cathode active material (NMC)
- Equipment
- intensive mixer and continuous kiln with ceramic trays
- Why it matters
- Firing is the step where the final chemical make-up of the cathode forms. vdma.org · secondary
- Source
- osti.gov · primary, read 2026-11-09
- 4
Graphitising the anode material
Coke and pitch are mixed hot, then baked in an electric furnace at extreme heat until the carbon orders itself into graphite.
Detail
- Goes in
- coke, pitch
- Comes out
- synthetic graphite
- Equipment
- intensive mixer or kneader, Acheson furnace
- Why it matters
- The heat is what lines the carbon up into the layered structure that can take in lithium. · our reading
- Numbers
- graphitising temperature: 1800 to 3000 degrees C (vdma.org · secondary)
- Source
- vdma.org · secondary, read 2026-11-09
Not published (3)
- which cathode the humanoid packs use is unresolved (the cell part: 4.2 V class, not LFP), so the NMC route is shown as the example Argonne models; the LFP and LCO routes are not opened
- natural graphite (shaping, purifying, coating): not opened here
- country shares of cathode and graphite production: no source read at this step; the battery map traces this chain
Who makes it, by country6 on the index
- United States2
- Japan2
- China1
- South Korea1
By result
- OSC: Allied owner4
- OSC: Owner unclear1
- OSC: Covered-nation owner1
- No record0
Results under OSC foreign influence. What each result means
Where they are
Makers on the index
All 6 on the map →- AltairnanoReno, United StatesOSC: Owner unclear
- Amprius TechnologiesFremont, United StatesOSC: Allied owner
- Gotion High-tech Co. Ltd.Hefei, ChinaOSC: Covered-nation owner
- Samsung SDI Co. Ltd.Yongin (Gyeonggi-do), South KoreaOSC: Allied owner
- Shin-Etsu ChemicalTokyo, JapanOSC: Allied owner
- Toshiba Corporation (SCiB LTO)Tokyo, JapanOSC: Allied owner